DrWesley Dose
Sydney Horizon Fellow (Senior Lecturer)
Faculty of Science
Orcid identifier0000-0003-3850-0505 (opens in a new tab)
- Sydney Horizon Fellow (Senior Lecturer)Faculty of Science
RESEARCH OUTPUTS
1-25 out of 108
- JOURNAL ARTICLEOperando characterisation of SEI formation in Ni-Rich lithium-ion cells to explore ethylene carbonate-free electrolyte systemsOct 2026Energy Storage Materials91:105516ElsevierCo-authors:
- Fordham A,
- Frost B,
- Jackowska R
DOIDOI: 10.1016/j.ensm.2026.105516 (opens in a new tab)
The pursuit of high-energy lithium-ion batteries (LIBs) has driven the adoption of Ni-rich layered oxides such as NMC811, but their reactivity with conventional ethylene carbonate (EC)-based electrolytes leads to interfacial instability and performance loss. Here, we systematically investigate how electrolyte composition and additives influence the formation and stability of the solid electrolyte interphase (SEI) in single-crystal NMC811‖graphite cells. Using commercial-grade pouch cells under a consistent formation protocol, we combine operando acoustic emission (AE) and electrochemical atomic force microscopy (EC-AFM) with complementary electrochemical and structural characterisation to probe SEI formation in real time. We first assess common additives in EC-containing electrolytes, then progressively reduce EC content, and finally introduce SEI-forming additives into EC-free electrolytes. Our results showed that while EC promotes SEI growth on graphite, it also accelerates parasitic reactions at the Ni-rich cathode, resulting in limited gains in cycling stability. Among the formulations examined, the 10% FEC delivered the best overall performance; this concentration was selected based on prior literature rather than systematic optimisation, which will be addressed in future work. This work demonstrates the dual role of EC in Ni-rich systems and highlights how correlative operando methods can guide rational electrolyte design for long-lived, high-energy LIBs. - PREPRINTAcoustic Emission to Provide Early Warning Detection of Lithium-Ion Battery Thermal Runaway7 Sep 2026ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Fordham A,
- Kesuma I,
- Dore T
DOIDOI: 10.26434/chemrxiv.15008458/v1 (opens in a new tab)
- JOURNAL ARTICLEDecoding MnO2 redox chemistry from mechanistic ambiguity to design principles for aqueous Zn-ion batteries11 Jun 2026Nature Communications17(1):7433Springer NatureCo-authors:
- Shang Y,
- Saha S,
- Wen H
DOIDOI: 10.1038/s41467-026-74350-z (opens in a new tab)
Manganese dioxide (MnO2) is a leading positive electrode candidate for aqueous zinc-ion batteries, combining safety, high voltage, low cost, and sustainability for grid-scale storage. However, its practical development remains restricted by poor reversibility, rooted in an unresolved mechanistic debate spanning over a decade. Here, we combine operando characterizations, multimodal spectroscopic analyses, and theory to establish a unified picture: proton-primed MnO2 dissolution and subsequent redeposition as nanocrystalline and disordered MnOx nanosheets, coexisting with reversible proton intercalation in parent MnO2 and predominantly in deposited MnOx, forming a dual redox mechanism. pH-driven insulating byproduct precipitation emerges as a significant kinetic barrier that limits deep dissolution and capacity utilization. Guided by these insights, we introduce surface activation and architectural design strategies toward mitigating kinetic barriers, enabling enhanced capacity and stability in both Swagelok and pouch-type cells. By reconciling mechanistic ambiguity and translating it into actionable design principles, this work demonstrates a framework for developing durable Mn-based positive electrodes for sustainable energy storage. - JOURNAL ARTICLEOptofluidic Raman Analysis and Capacity Recovery in Li‐ion CellsJun 2026Advanced Materials Technologies11(12)WileyCo-authors:
- Miele E,
- Dose WM,
- Davidson IAK
DOIDOI: 10.1002/admt.202502292 (opens in a new tab)
ABSTRACT Battery performance degradation arises from multifactorial and complex electrochemical processes involving all the battery components. Therefore, identifying and mitigating/suppressing the main degradation mechanisms is essential for deploying these technologies. Such a holistic understanding requires advanced and dedicated analytical tools as well as effective strategies to recover battery capacity, extend battery life, and facilitate second‐life use and recycling of devices. Here, we develop a set of optical and microfluidic methodologies that enable operando chemical analysis of liquid electrolytes using Raman spectroscopy. We demonstrate that our methods have minimal perturbation on device operation and can be readily embedded in standard manufacturing processes. A bi‐directional microfluidic access port allows the extraction and reinjection of carbonate‐based electrolytes for analysis over hundreds of electrochemical cycles. Our data show that lithium salt anion (PF 6 − ) degradation is a major source of electrolyte degradation and capacity loss in industrially relevant Li‐ion pouch cells (Ni‐rich layered cathodes (NMC811), and graphite anodes). The effects are particularly strong when cycled to an upper‐cut voltage of 4.3 V. Finally, we demonstrate that battery capacity loss can be partially reversed by re‐infusing pristine, uncycled electrolyte via an integrated microfluidic access port. This strategy not only mitigates degradation and extends battery life but also offers a practical pathway toward second‐life applications and adaptable cell chemistries for future battery technologies. - JOURNAL ARTICLEMitigating Electrochemical Isolation in Ni‐Rich Layered Cathodes for Durable Solid‐State BatteriesApr 2026Advanced Science13(19):e18327WileyCo-authors:
- Bhadra A,
- Brunisholz M,
- Rawal A
DOIDOI: 10.1002/advs.202518327 (opens in a new tab)
Cathode-solid electrolyte (SE) interfacial instability poses a major challenge for achieving stable and high-power operations in all-solid-state batteries, which promise superior energy density, thermal stability, and safety over the current Li-ion technology. For technologically important Ni-rich NMCs (LiNi<sub>x</sub>Mn<sub>y</sub>Co<sub>z</sub>O<sub>2</sub> or NMCxyz; x/y/z: Ni/Mn/Co stoichiometry) paired with sulfide SEs, redox-mediated instability of the SE is often blamed for rapid cathode deterioration. Here, in-depth spectroscopic and electrochemical analyses of Ni-rich NMCs with a promising sulfide SE reveal hitherto unrecognized electrochemical isolation of active NMC particles driven by rapid interfacial degradations, sparking accelerated capacity fading and poor thermal stability. Introducing a functionalized conductive carbon into the cathode suppresses sulfide SE degradation into reactive polysulfides that drive NMC deterioration. Consequently, NMC622 and NMC811-based cells display high active material utilization, enhanced stability, attractive rate capability and thermal resilience - illustrated by 1C (1C: 160 mA g<sup>-1</sup>) capacity of ∼150 mAh g<sup>-1</sup>, 5C rate retention of 95% after 500 cycles with high active loading (≥12 mg cm<sup>-2</sup>), and an average Coulombic efficiency of 99.8% even for high-temperature cycling. This study uncovers a critical performance degradation pathway in a key cathode-SE pairing and presents a scalable strategy for its in situ regulation, enabling significant performance gains. - JOURNAL ARTICLEUtilising acoustic techniques to improve understanding of the formation process in sodium-ion batteries9 Feb 2026EES Batteries2(1):253-269Royal Society of Chemistry (RSC)Co-authors:
- Fordham A,
- Wee D,
- Owen RE
DOIDOI: 10.1039/d5eb00170f (opens in a new tab)
Operando acoustic techniques enabling non-invasive monitoring of SEI formation and performance in sodium-ion batteries. Sodium-ion batteries (NIBs) offer a more sustainable and cost-effective alternative to lithium-ion batteries (LIBs), but challenges related to the formation process and the impact of electrolyte additives on the solid electrolyte interphase (SEI) remain underexplored. Moreover, current SEI diagnostic tools are often prohibitively expensive, limiting broader adoption. This work investigates operando , non-invasive acoustic techniques – combining passive acoustic emission (AE) and active ultrasonic testing (UT) – to monitor SEI formation in NaMn 0 . 39 Fe 0 . 31 Ni 0 . 22 Zn 0 . 08 O 2 /hard carbon (HC) pouch cells using four electrolyte formulations: a baseline of 1 M NaPF 6 in 1 : 1 EC : DMC, and three with additives (5 wt% fluoroethylene carbonate (FEC), vinylene carbonate (VC), or both). Identical formation protocols were applied, with SEI evolution monitored via AE and UT, and correlated with a range of characterisation techniques including operando gas volume measurements, three-electrode d Q /d V analysis, and X-ray CT. Bespoke machine learning algorithms were developed to interpret acoustic signals. Results revealed incomplete SEI passivation across all formulations, evidenced by ongoing gas evolution and high irreversible capacity loss after three formation cycles. The behaviour in formation was reflected in the long-term cycling results: FEC delivered the best performance, VC alone was less effective, and cells without additives performed worst. These findings highlight the importance of tailored additive selection when using NaPF 6 in NIBs. This work demonstrates that AE and UT provide a viable, low-cost solution for real-time SEI monitoring, offering mechanistic insight previously accessible only through more complex and costly techniques. - PREPRINTOperando Characterisation of SEI Formation in Ni-Rich Lithium-Ion Cells to Explore Ethylene Carbonate-Free Electrolyte Systems8 Feb 2026ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Fordham A,
- Frost B,
- Jackowska R
DOIDOI: 10.26434/chemrxiv.10002013/v1 (opens in a new tab)
- JOURNAL ARTICLEThe interplay between stack pressure, mechanical expansion and degradation pathways in lithium-ion batteries2026Nature Energy11(7):1032-1042Springer NatureCo-authors:
- Wang H,
- Wang R,
- O’Keefe CA
DOIDOI: 10.1038/s41560-026-02087-6 (opens in a new tab)
While electrochemical degradation mechanisms in lithium-ion batteries are well studied, the influence of mechanical factors remains poorly understood. Here we introduce a high-precision stack-pressure control and dilatometry tool to apply a uniform and constant stack pressure on electrodes independent of electrode swelling. By increasing stack pressure fourfold over typical initial values, we double the lifetime of graphite ‖ LiNi0.8Mn0.1Co0.1O2 cells, an industrially relevant battery chemistry, without altering active materials or electrolytes. This suggests that many lithium-ion batteries operate under sub-optimal stack-pressure conditions, leading to curtailed lifetimes. We demonstrate that different degradation mechanisms emerge outside the optimal pressure window: low stack pressure accelerates cathode cracking, whereas high pressure promotes lithium plating. Our findings highlight coupled mechanical–electrochemical degradation mechanisms and identify stack-pressure optimization as a practical solution for increasing cycling stability. - JOURNAL ARTICLERevealing How Silicon Oxide Accelerates Calendar Ageing of Commercial 21700 Nickel-Rich Lithium-Ion Cells1 Sep 2025Journal of The Electrochemical Society172(9):090505The Electrochemical SocietyCo-authors:
- Majherova V,
- Fiamegkou E,
- Nakhanivej P
DOIDOI: 10.1149/1945-7111/adfe98 (opens in a new tab)
This study investigates the calendar ageing behaviour of NMC811//SiOx-graphite 21700 cylindrical cells (LGM 50), which were held at varying states of charge (SoC), for up to 70 weeks at 4 different temperatures. Throughout the ageing study, capacity and internal resistance were monitored, and significant capacity loss over time, with greater loss at high SoC and temperature, were observed. A combination of electrochemical testing and post-mortem characterisation techniques point to the anode, more specifically, the silicon-oxide particles, as the driver of capacity fade through unstable solid-electrolyte interface dynamics, leading to the gradual loss of lithium inventory. Despite the greatest capacity loss being at ∼80% SoC and the apparent improvement in capacity retention at higher SoCs, i.e. the “spoon-shape effect,” the degradation is most pronounced at 100% SoC, driven by the instability of the silicon-oxide SEI. This is demonstrated by post-calendar ageing cycling of the cells, where those aged at 100% SoC degraded at a faster rate than 80% SoC. Higher temperatures and SoC levels significantly accelerate calendar ageing degradation of NMC//SiOx-graphite cylindrical cells.Cells aged at 80% SoC showed larger capacity fade then cells stored at 100% SoC - this increase in capacity was found to be as a result of lithium inventory release due to more degradation.Despite the increase in capacity, more significant degradation was observed in cells aged at 100% SoC through advanced characterisation and cycling tests.Post-mortem analysis—including CT scanning, neutron and X-ray diffraction, SIMS/EDS, and differential voltage analysis—revealed that capacity fade is primarily attributed to the loss of active material in the anode and lithium inventory, especially associated with the presence of silicon. Higher temperatures and SoC levels significantly accelerate calendar ageing degradation of NMC//SiOx-graphite cylindrical cells. Cells aged at 80% SoC showed larger capacity fade then cells stored at 100% SoC - this increase in capacity was found to be as a result of lithium inventory release due to more degradation. Despite the increase in capacity, more significant degradation was observed in cells aged at 100% SoC through advanced characterisation and cycling tests. Post-mortem analysis—including CT scanning, neutron and X-ray diffraction, SIMS/EDS, and differential voltage analysis—revealed that capacity fade is primarily attributed to the loss of active material in the anode and lithium inventory, especially associated with the presence of silicon. - PREPRINTUtilising Acoustic Techniques to Improve Understanding of the Formation Process in Sodium-ion Batteries25 Aug 2025ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Fordham A,
- Wee D,
- Owen R
DOIDOI: 10.26434/chemrxiv-2025-gcffl (opens in a new tab)
- JOURNAL ARTICLESinglet oxygen is not the source of ethylene carbonate degradation in nickel-rich Li-ion cells29 Jul 2025Energy & Environmental Science18(15):7603-7609Royal Society of Chemistry (RSC)Co-authors:
- McNulty RC,
- Jones KD,
- Denison BMG
DOIDOI: 10.1039/d5ee00956a (opens in a new tab)
Photochemical assessment shows ethylene carbonate does not react with singlet oxygen, indicating degradation within nickel-rich cells follows an alternative route. Nickel-rich intercalation electrodes ( i.e. Ni 0.8 Mn 0.1 Co 0.1 O 2 ) are seeing widespread adoption in high-performance lithium-ion batteries due to their high energy density and reduced need for cobalt. However, as nickel content increases, so too does the rate of cell capacity fade, which in part has been assigned to reactions between ethylene carbonate (EC) and reactive oxygenic species formed at the surface of nickel-rich electrodes. In particular, singlet oxygen ( 1 O 2 ) has long been suspected as a primary source of ethylene carbonate degradation and has been proposed to drive its conversion to either vinylene carbonate, a graphite stabilising additive, or to complete oxidation products such as CO 2 , and protic species ( i.e. H 2 O, H 2 O 2 ) that accelerate cell failure. Contrary to this understanding, we show using online mass spectrometry and quantitative 1 H NMR spectroscopic analysis that ethylene carbonate is stable in the presence of photocatalytically generated 1 O 2 . Furthermore, this study indicates the use of rose bengal as a photocatalyst to study ethylene carbonate reactivity with 1 O 2 may lead to unexpected side-reactions under operationally-relevant conditions, producing misleading results. We conclude that the choice of photocatalyst is critical when assessing degradation with 1 O 2 for battery applications. Despite eliminating the direct reaction of 1 O 2 with EC as a source of degradation, ethylene carbonate to vinylene carbonate conversion is still found to occur in cells. We demonstrate that vinylene carbonate production begins before gas release from the positive electrode. These findings show that degradation driven by 1 O 2 reaction with EC is unlikely to be an important factor at nickel-rich intercalation electrodes highlighting the need for the community to explore alternative degradation pathways in nickel-rich lithium-ion batteries. - JOURNAL ARTICLEChemical Degradation Routes of Electrolytes in Nickel-Rich Lithium-Ion Batteries: Where Does It All Begin?11 Jul 2025ECS Meeting AbstractsMA2025-01(3):313The Electrochemical SocietyCo-authors:
- Jones KD,
- McNulty RC,
- Denison BMG
DOIDOI: 10.1149/ma2025-013313mtgabs (opens in a new tab)
As global demand for electrification increases, the availability and versatility of our battery systems need to advance.1 Nickel-rich electrodes such as LiNi0.8Mn0.1Co0.1O2 (NMC811) or LiNiO2 (LNO) reduce reliance on complicating cobalt-rich electrodes,2 while delivering higher capacity than that of LiCoO2. However, nickel-rich materials suffer from lattice instability and can produce reactive oxygenic species, such as singlet oxygen, that are proposed to react with the electrolyte. It has been speculated that many of the degradation modes in nickel-rich electrodes originate from decomposition of electrolyte components, generating antagonistic intermediates, often protic (i.e HF or H2O), leading to cell failure.3 The initialisation of the ethylene carbonate-based electrolyte degradation sequence has been proposed to be driven by electrochemical oxidation,4 chemical dehydrogenation by high state of charge metal oxides,5 and/or by direct C-H insertion from singlet oxygen released from the lattice at higher voltages,6,7 all leading to unstable or protic by-products within the cell, exacerbating failure. Here we consider how the surface chemistry of the nickel-rich electrodes changes during cycling and how this may impact degradation. These events are compared to the potentials at which oxygen is released from the cell, with a range of organic-analytical-electrochemistry techniques to understand electrolyte degradation at nickel-rich electrodes. We have successfully identified vinylene carbonate in extracted electrolyte, among other components, and assessed the influence of in situ formation on long-term cell cycling. Finally, we consider how vinylene carbonate forms within the cell and provide clarity as to the major bad actors responsible for ethylene carbonate degradation in nickel-rich lithium-ion batteries. [1] Booth, G. A., et al., APL Mater., 9, 109201 (2021); [2] Olivetti, E. A., et al., Joule., 1, 229 (2017); [3] Cui, Z., et al., Angew. Chem. Int. Ed., 62, e202307243 (2023); [4] Jung, R., et al., J. Electrochem. Soc., 164 A1361 (2017); [5] Zhang, Y., et al., Energy Environ. Sci., 13, 183 (2020); [6] Freiberg, A. T. S., et al., J. Phys. Chem. A., 122, 8828 (2018); [7] Rinkel, B. L. D., et al., Energy Environ. Sci., 15, 3416 (2022) Figure 1 - JOURNAL ARTICLEThe Impact of Singlet Oxygen Release on Ethylene Carbonate-Based Lithium-Ion Electrolytes11 Jul 2025ECS Meeting AbstractsMA2025-01(2):117The Electrochemical SocietyCo-authors:
- Denison BMG,
- McNulty RC,
- Jones KD
DOIDOI: 10.1149/ma2025-012117mtgabs (opens in a new tab)
The electrification of the transport sector calls for batteries with higher capacity and power capabilities. Thus, nickel-rich positive electrode materials, specifically LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), have seen a drastic increase in popularity. 1 , 2 However, NMC811 suffers decreased cycle life compared to lower nickel content electrodes due to its poorer structural stability, and increased reactivity towards commercial electrolytes consisting of organic carbonates and LiPF 6 , with ethylene carbonate (EC) being a common component. The proposed degradation routes of EC are by reactions at the nickel surface at high states-of charge (>80%) and with singlet oxygen ( 1 O 2 ) released from the lattice at high voltages, yielding vinylene carbonate (VC), an SEI stabilising additive, as a primary product. 3 , 4 , 5 Unfortunately, protic byproducts ( i.e. H + , H 2 O) are simultaneously formed resulting in a cascade of reactions, generating key antagonists such as HF, and ultimately contributing to cell failure. 6 , 7 Herein, a multidisciplinary approach combining aspects of analytical, battery, and organic chemistry will be described to determine if 1 O 2 is the cause of in-situ VC formation and subsequent cell failure mechanisms. VC formation in NMC811 full cells is confirmed at potentials as low as 3.9 V and demonstrates a dependence on upper cut off voltage. Additionally, commercial electrolytes with and without VC as an additive are shown to have comparable long-term cycling performance, bringing the requirement of VC in Ni-rich full cells into question. Finally, 1 O 2 reactivity with EC is reviewed by on-line mass spectrometry and 1 H NMR spectroscopy, where EC is found to be inert to 1 O 2 , eliminating it as a source of EC degradation. [1] Y. Ding, Z. P. Cano, A. Yu, J. Lu and Z. Chen, Electrochem. Energy Rev. , 2019, 2 , 1–28. [2] W. Li, E. M. Erickson and A. Manthiram, Nat. Energy , 2020, 5 , 26–34. [3] B. L. D. Rinkel, J. P. Vivek, N. Garcia-Araez and C. P. Grey, Energy Environ. Sci. , 2022, 15 , 3416–3438. [4] A. T. S. Freiberg, M. K. Roos, J. Wandt, R. de Vivie-Riedle and H. A. Gasteiger, J. Phys. Chem. A , 2018, 122 , 8828–8839. [5] Y. Zhang, Y. Katayama, R. Tatara, L. Giordano, Y. Yu, D. Fraggedakis, J. G. Sun, F. Maglia, R. Jung, M. Z. Bazant and Y. Shao-Horn, Energy Environ. Sci. , 2020, 13 , 183–199. [6] S. Wiemers-Meyer, M. Winter and S. Nowak, Phys. Chem. Chem. Phys. , 2016, 18 , 26595–26601. [7] J. L. Tebbe, T. F. Fuerst and C. B. Musgrave, J. Power Sources , 2015, 297 , 427–435. Figure 1 - JOURNAL ARTICLEDegradation Pathways in Lithium‐Ion Batteries with Ethylene Carbonate‐Free ElectrolytesJun 2025Advanced Energy Materials15(22)WileyCo-authors:
- Terreblanche JS,
- Luo T,
- Piper LFJ
DOIDOI: 10.1002/aenm.202404427 (opens in a new tab)
Abstract The development of stable electrolyte solutions is critical for improving the lifetime and performance of lithium‐ion batteries (LIBs). Electrolyte instability is a prominent issue with many next‐generation electrode materials, such as Ni‐rich cathodes, with recent reports identifying ethylene carbonate (EC) as a bad actor at the cathode surface. Herein, electrochemical methods, operando pressure measurements, and post‐mortem X‐ray and solution NMR studies are combined to investigate electrolyte and interfacial degradation phenomena in Ni‐rich LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)/graphite full cells with EC‐containing and EC‐free electrolytes. One key finding is that the mechanism for improved performance in EC‐free electrolyte–1.5 M LiPF 6 in ethyl methyl carbonate (EMC) with 10 wt.% fluoroethylene carbonate (FEC)–arises from improved stability at both electrode‐electrolyte interfaces. The EC‐free electrolyte is found to suppress lattice oxygen release and reduce surface layer formation at NMC, leading to improved ion transport into the cathode particles, suppressed electrolyte solvent oxidation reactions, less formation and crossover of species that disrupt the graphite solid electrolyte interphase (SEI), and ultimately improved capacity retention. These insights are helpful in understanding and mitigating degradation in LIBs with Ni‐rich cathodes. - PREPRINTSurface oxygen drives electrolyte degradation at Ni-rich battery cathodes15 May 2025Research SquareSpringer NatureCo-authors:
- Stephens I,
- Thornton D,
- Seymour I
DOIDOI: 10.21203/rs.3.rs-6512009/v1 (opens in a new tab)
- PREPRINTRevealing how silicon oxide accelerates calendar ageing of commercial 21700 nickel-rich lithium-ion cells28 Apr 2025ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Majherova V,
- Fiamegkou E,
- Nakhanivej P
DOIDOI: 10.26434/chemrxiv-2025-vndg1 (opens in a new tab)
- PREPRINTFirst Observation and Mitigation of Ni-Leaching Mediated Degradation to Enhance Stability of Ni-rich Layered Cathodes in Solid-State Batteries19 Mar 2025ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Bhadra A,
- Otabil Bonsu J,
- Brunisholz M
DOIDOI: 10.26434/chemrxiv-2025-r1nf2 (opens in a new tab)
- PREPRINTDegradation pathways in lithium-ion batteries with ethylene carbonate-free electrolytes16 Jan 2025ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Terreblanche JS,
- Luo T,
- Piper LFJ
DOIDOI: 10.26434/chemrxiv-2024-nmnr8-v4 (opens in a new tab)
- JOURNAL ARTICLEListening to Batteries: Utilising Acoustic Characterisation Techniques to Optimise Formation Cycle Protocols in Lithium-Ion Batteries22 Nov 2024ECS Meeting AbstractsMA2024-02(4):479The Electrochemical SocietyCo-authors:
- Fordham A,
- Owen RE,
- Dose WM
DOIDOI: 10.1149/ma2024-024479mtgabs (opens in a new tab)
The optimisation of the formation cycle in battery manufacturing plays a crucial role in driving the success of the electric revolution. The formation cycle, which involves the initial charging and discharging of lithium-ion batteries (LIB)s to stabilise their electrochemical processes, directly impacts the overall performance and longevity. 1 This formation process of LIBs is the most expensive and time-consuming step in the total battery pack cost and process, meaning it is a critical bottleneck in the manufacturing industry and requires substantial capital equipment to deliver reliably. 2,3 The long duration is required to ensure that a stable layer of surface interphase grows between the electrode and electrolyte, known as the Solid Electrolyte Interphase (SEI). A stable SEI layer is essential to minimise active lithium loss, electrolyte depletion and capacity fade over the lifetime of the battery, as well as mitigating safety issues within the cell and pack. 4 It is therefore vital to develop novel characterisation techniques to improve this formation process. Acoustic methods are one of the most promising diagnostic and characterisation techniques for batteries. The technique offers the potential for a real-time operando prediction of the State of Health (SoH), State of Charge (SoC) and State of Safety (SoS). 5–7 Broadly, acoustic techniques can be divided into Acoustic Emission (AE) and Ultrasonic Testing (UT) methods; each slightly differs in terms of purpose and experimental setup. Both techniques can detect the physical and electrochemical changes within the cell during usage such as gas formation and cracking. 8 In this work, conducted at UCL under the Faraday Institution's SafeBatt project, we use a combination of Acoustic Emission and pulse-echo Ultrasonic Testing in a novel dual-sensor approach. Utilising the sensors, we detect the growth of the solid electrolyte interphase (SEI) during the cell's formation cycle under different protocols and with varying additives. Additionally, we investigate the influence of this SEI layer on the long-term performance and State of Health (SoH) of the cell. We then developed bespoke formation protocols with voltage holds, using acoustic techniques to determine the point at which SEI formation finished and the corresponding success of the passivation layer. This technique can characterise how successfully a cell has formed based on the acoustic signals released, offering a low-cost, non-invasive, and non-destructive approach. We correlated the acoustic results to X-ray photoelectron spectroscopy (XPS), X-ray Computed Tomography, Scanning Electron Microscopy (SEM), Atomic Force Microscopy (AFM), and in-situ gas volume measurements to confirm the hypotheses made from the acoustic measurements. The results confirmed that as the C-rate increases, a greater amount of acoustic activity is observed, which is attributed to gas formation. Based on the acoustic emission (AE) activity, we were also able to determine the exact voltage at which chemical reactions occur in the electrode electrolyte interphase, including the point where the SEI was developing during the formation cycle. These findings demonstrate the potential for employing acoustic sensors in industry as an advanced characterisation technique to enhance the formation cycle process. References Alptekin, H., Pathan, T.S., Rashid, M., Walker, M., and Widanage, W.D. (2021). Active formation of Li-ion batteries and its effect on cycle life. Leißing, M., Horsthemke, F., Wiemers-Meyer, S., Winter, M., Niehoff, P., and Nowak, S. (2021). The Impact of the C-Rate on Gassing During Formation of NMC622 II Graphite Lithium-Ion Battery Cells. Batter. Supercaps 4 , 1344–1350. 10.1002/batt.202100056. Iii, D.L.W. (2019). Formation Challenges of Lithium-Ion Battery Manufacturing. Joule 3 , 2884–2888. 10.1016/j.joule.2019.11.002. Wu, J., Ihsan-Ul-Haq, M., Chen, Y., and Kim, J.K. (2021). Understanding solid electrolyte interphases: Advanced characterization techniques and theoretical simulations. Nano Energy 89 , 106489. 10.1016/j.nanoen.2021.106489. Bommier, C., Chang, W., Li, J., Biswas, S., Davies, G., Nanda, J., and Steingart, D. (2020). Operando Acoustic Monitoring of SEI Formation and Long-Term Cycling in NMC/SiGr Composite Pouch Cells. J. Electrochem. Soc. 167 , 020517. 10.1149/1945-7111/ab68d6. Robinson, J.B., Owen, R.E., Kok, M.D.R., Maier, M., Majasan, J., Braglia, M., Stocker, R., Amietszajew, T., Roberts, A.J., Bhagat, R., et al. (2020). Identifying Defects in Li-Ion Cells Using Ultrasound Acoustic Measurements. J. Electrochem. Soc. 167 , 120530. 10.1149/1945-7111/abb174. Fordham, A., Milojevic, Z., Giles, E., Du, W., Owen, R.E., Michalik, S., Chater, P.A., Das, P.K., Attidekou, P.S., Lambert, S.M., et al. (2023). Correlative non-destructive techniques to investigate aging and orientation effects in automotive Li-ion pouch cells. Joule 7 , 2622–2652. 10.1016/j.joule.2023.10.011. Fukushima, T., Kato, S., Kuwata, N., and Kawamura, J. (2014). In-Situ Acoustic Emission Study of Sn Anode in Li Ion Battery. ECS Trans. 62 , 215–222. 10.1149/06201.0215ecst. Figure 1 - JOURNAL ARTICLEUnderstanding Electrolyte Stability and Instability in Lithium-Ion Batteries with Nickel-Rich Cathodes22 Nov 2024ECS Meeting AbstractsMA2024-02(7):1039The Electrochemical SocietyCo-authors:
- Terreblanche JS,
- Luo T,
- Piper LF
DOIDOI: 10.1149/ma2024-0271039mtgabs (opens in a new tab)
Developing electrolyte solutions that are stable at the electrode-electrolyte interfaces is critically important to enable high performance lithium-ion batteries. The discovery in the early 1990s that a mixture of ethylene carbonate (EC) and alkyl carbonate(s) could passivate graphite led to a step change in the cell energy density, 1,2 and modern batteries still retain this skeleton electrolyte formulation and graphite anode combination. However, as the battery industry shifts to nickel-rich layered oxide cathodes for lower cost and higher energy density cells, 3,4 an incompatibility between EC-containing electrolytes and the cathode is starting to be revealed. This is driving research efforts to, firstly, understand the chemical reactions at the nickel-rich cathode-electrolyte interface 5-9 and, secondly, explore new EC-free electrolyte solutions. 10-13 Here we examine the dominant degradation phenomena in nickel-rich NMC/graphite full cells with EC-containing and EC-free electrolytes. We combine a range of methods including cell cycling, operando pressure measurements, OEMS, XPS, XRF, and solution NMR to understand the behaviour of the two electrolyte systems throughout the full cell. The results of these studies will be discussed in conjunction with their implications for further development of compatible electrolytes for advanced lithium-ion battery chemistries. References: Xu, Nat. Energy, 2021, 6 , 763. Fujimoto, N. Yoshinaga, K. Ueno, N. Furukawa, T. Nohma, M. Takahashi, Japanese patent, 3,229,635, 1991. Xu, X. Liu, A. Daali, R. Amine, Z. Chen, K. Amine, Adv. Funct. Mater., 2020, 30 , 2004748 Li, E.M. Erickson, A. Manthiram, Nat. Energy, 2020, 5 , 26. Wandt, A.T.S. Freiberg, A. Ogrodnik, H.A. Gasteiger, Mater. Today, 2018, 21 , 825. T.S. Freiberg, M.K. Roos, J. Wandt, R. de Vivie-Riedle, H.A. Gasteiger, J. Phys. Chem. A, 2018, 122 , 8828. Zhang, Y. Katayama, R. Tatara, L. Giordano, Y. Yu, D. Fraggedakis, J.G. Sun, F. Maglia, R. Jung, M.Z. Bazant, Y. Shao-Horn, Energy Environ. Sci. 2020, 13 , 183. M. Dose, I. Temprano, J.P. Allen, E. Bjorklund, C.A. O'Keefe, W. Li, B.L. Mehdi, R.S. Weatherup, M.F.L. De Volder, C.P. Grey, ACS Appl. Mater. Interfaces, 2022, 14 , 13206. M. Dose, W. Li, I. Temprano, C.A. O’Keefe, B.L. Mehdi, M.F.L. De Volder, C.P. Grey, ACS Energy Lett., 2022, 7 , 3524. Xia, R. Petibon, D. Xiong, L. Ma, J.R. Dahn, J. Power Sources, 2016, 328 , 124. Petibon, J. Xia, L. Ma, M.K.G. Bauer, K.J. Nelson, J.R. Dahn, J. Electrochem. Soc. 2016, 163 , A2571. Li, A. Dolocan, J. Li, Q. Xie, A. Manthiram, Adv. Energy Mater., 2019, 9 , 1901152. Pan, Z. Cui, M. Yi, Q. Xie, A. Manthiram, Adv. Energy Mater., 2022, 12 , 2103806. Figure 1 - PREPRINTDegradation pathways in lithium-ion batteries with ethylene carbonate-free electrolytes26 Sep 2024ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Terreblanche JS,
- Luo T,
- Piper LFJ
DOIDOI: 10.26434/chemrxiv-2024-nmnr8-v3 (opens in a new tab)
- PREPRINTDegradation pathways in lithium-ion batteries with ethylene carbonate-free electrolytes20 Sep 2024ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Terreblanche JS,
- Luo T,
- Piper LFJ
DOIDOI: 10.26434/chemrxiv-2024-nmnr8-v2 (opens in a new tab)
- PREPRINTElectrolyte stability and instability in lithium-ion batteries24 May 2024ChemRxivAmerican Chemical Society (ACS)Co-authors:
- Terreblanche JS,
- Luo T,
- Piper LFJ
DOIDOI: 10.26434/chemrxiv-2024-nmnr8 (opens in a new tab)
- JOURNAL ARTICLEOrigins and Importance of Intragranular Cracking in Layered Lithium Transition Metal Oxide Cathodes13 May 2024ACS Applied Energy Materials7(9):3945-3956American Chemical Society (ACS)Co-authors:
- Morzy JK,
- Dose WM,
- Vullum PE
DOIDOI: 10.1021/acsaem.4c00279 (opens in a new tab)
Li-ion batteries have a pivotal role in the transition toward electric transportation. Ni-rich layered transition metal oxide (LTMO) cathode materials promise high specific capacity and lower cost but exhibit faster degradation compared with lower Ni alternatives. Here, we employ high-resolution electron microscopy and spectroscopy techniques to investigate the nanoscale origins and impact on performance of intragranular cracking (within primary crystals) in Ni-rich LTMOs. We find that intragranular cracking is widespread in charged specimens early in cycle life but uncommon in discharged samples even after cycling. The distribution of intragranular cracking is highly inhomogeneous. We conclude that intragranular cracking is caused by local stresses that can have several independent sources: neighboring particle anisotropic expansion/contraction, Li- and TM-inhomogeneities at the primary and secondary particle levels, and interfacing of electrochemically active and inactive phases. Our results suggest that intragranular cracks can manifest at different points of life of the cathode and can potentially lead to capacity fade and impedance rise of LTMO cathodes through plane gliding and particle detachment that lead to exposure of additional surfaces to the electrolyte and loss of electrical contact. - JOURNAL ARTICLEMicrostructures of layered Ni-rich cathodes for lithium-ion batteries7 May 2024Chemical Society Reviews53(9):4707-4740Royal Society of Chemistry (RSC)Co-authors:
- Lu J,
- Xu C,
- Dose W
DOIDOI: 10.1039/d3cs00741c (opens in a new tab)
Millions of electric vehicles (EVs) on the road are powered by lithium-ion batteries (LIBs) based on nickel-rich layered oxide (NRLO) cathodes, and they suffer from a limited driving range and safety concerns. Increasing the Ni content is a key way to boost the energy densities of LIBs and alleviate the EV range anxiety, which are, however, compromised by the rapid performance fading. One unique challenge lies in the worsening of the microstructural stability with a rising Ni-content in the cathode. In this review, we focus on the latest advances in the understanding of NLRO microstructures, particularly the microstructural degradation mechanisms, state-of-the-art stabilization strategies, and advanced characterization methods. We first elaborate on the fundamental mechanisms underlying the microstructural failures of NRLOs, including anisotropic lattice evolution, microcracking, and surface degradation, as a result of which other degradation processes, such as electrolyte decomposition and transition metal dissolution, can be severely aggravated. Afterwards, we discuss representative stabilization strategies, including the surface treatment and construction of radial concentration gradients in polycrystalline secondary particles, the fabrication of rod-shaped primary particles, and the development of single-crystal NRLO cathodes. We then introduce emerging microstructural characterization techniques, especially for identification of the particle orientation, dynamic changes, and elemental distributions in NRLO microstructures. Finally, we provide perspectives on the remaining challenges and opportunities for the development of stable NRLO cathodes for the zero-carbon future.